The wear takes place when two material load on slide one over the other. The wear resistance of a material is measured by testing "Pin-on-Disc" to analyzing a material loss. All this on a strict control of loads, temperatures, speeds and roughness of surfaces. For more information contact our consultancy department.
For more information contact our consulting department.
*These data will be used for comparison and support in the material choice. We are not responsible for its use.
| Product | Material | Value (20 = Better) |
|---|---|---|
| Ertalyte TX | Polyethylene Terephtalate | 20 |
| Techtron HPV PPS | Polyphenylene Sulfide PPS | 20 |
| Duratron T4301 PAI | Polyamide-imide PAI | 20 |
| Ketron Peek HPV | Polyetheretherketone Peek | 20 |
| Duratron T4203 PAI | Polyamide-imide PAI | 19 |
| Nylatron 703 XL | Polyamide | 19 |
| Ketron Peek 1000 | Polyetheretherketone Peek | 19 |
| Ertalyte | Polyethylene Terephtalate | 19 |
| Ertalon LFX | Polyamide | 18 |
| Duratron PBI | Polybenzimidazole PBI | 18 |
| Ketron Peek CA30 | Polyetheretherketone Peek | 18 |
| Nylatron GSM | Polyamide | 17 |
| Ketron Peek GF30 | Polyetheretherketone Peek | 17 |
| Nylatron GS | Polyamide | 17 |
| Ertalon 6 XAU + | Polyamide | 16 |
| Ertalon 6 SA | Polyamide | 16 |
| Ertalon 66 SA | Polyamide | 16 |
| Ertalon 6 PLA | Polyamide | 16 |
| Ertalon 4.6 | Polyamide | 16 |
| Nylatron MC901 | Polyamide | 16 |
| Ertalon 66 GF30 | Polyamide | 15 |
| Ertacetal C | Polyacetal | 14 |
| PC 1000 | Polyacarbonat PC | 4 |
| PEI 1000 | Polyetherimide - PEI | N/A |
| PSU 1000 | Polysulfone PSU | N/A |